Why Hairline Cracks in Concrete | Types of Cracks in Concrete
What Is Concrete Topping | Topping Slab Definition | Types of Topping Slab | Advantages & Disadvantage of Topping Slab
What Is a Concrete Mixer | Types of Concrete Mixer | Specifications of the Concrete Mixer | How to Mix Concrete in a Mixer
What Is Concrete Screed | Concrete Screed Specifications | Characteristics of Concrete Screed | Advantages & Disadvantages of Concrete Screed
What Is Modulus of Rupture | What Is Flexural Modulus | What Is Flexural Stress | Flexural Strength of Concrete | Bending Modulus | What Is Flexural Strength
Add a very less amount of water content in the mix of the concrete or use chemical admixtures to show that demand for water gets reduced and required workability is also achieved.
Design the concrete mix properly add more amount of cement in the concrete mix.
Proper measure and method of mixing should be used to reduce bleeding in the concrete.
Light: When the detected area of the concrete measures less than 150 mm in any direction or less than 25 mm in depth. This will be considered as a light spalling of concrete.
Medium: When the defected area concrete measures between 150mm to 300mm in any direction or between 25mm and 50mm in depth. This will be considered as a medium spalling of concrete.
Severe: When the defected area of concrete measures between 300mm to 600mm in any direction or between 50mm and 100mm in depth. It will be considered as severe spalling of concrete.
Very severe: When the defected area of the concrete more than 600 mm in any direction or greater than 100 mm in depth. This will be considered as the very severe spalling of concrete.
Light: The light scaling of the concrete occurs When there is a Loss of surface mortar up to 5mm depth without any exposure of coarse aggregates.
Medium: The medium scaling of the concrete occurs When there is a Loss of surface mortar up to 6 to 10 mm depth with exposure of some coarse aggregates.
Severe: The severe scaling of the concrete occurs when there is a loss of surface mortar up to 11 mm to 20 mm with aggregate particles standing out from the concrete.
VerySevere: The very severe scaling of the concrete occurs when there is a loss of mortar and aggregate particles to a depth greater than 20 mm.